304 Stainless Steel

This alloy is the most commonly used type of stainless steel sheet. That’s because it’s weldable, machineable and has good corrosion resistance. Some common applications of 304 stainless steel sheeting include food processing equipment, heat exchangers, springs, chemical containers, and more. Can be used in temperatures up to 1800°F.

Product introduction

Stainless steel 304 and stainless steel 304L are also known as 1.4301 and 1.4307 respectively. 304 is the most versatile and widely used stainless steel. It is still sometimes referred to by its old name 18/8 which is derived from the nominal composition of 304 being 18% chromium and 8% nickel. 304 stainless steel is an austenitic grade that can be severely deep drawn. This property has resulted in 304 being the dominant grade used in applications like sinks and saucepans. 304L is the low carbon version of 304. It is used in heavy gauge components for improved weldability.  304H, a high carbon content variant, is also available for use at high temperatures. 

 

Available in form of

STAINLESS STEEL 304 SHEET

STAINLESS STEEL 304 PLATE

STAINLESS STEEL 304 COIL

STAINLESS STEEL 304  STRIP

STAINLESS STEEL 304 FLAT

STAINLESS STEEL 304 SHIM

STAINLESS STEEL 304 CIRCLE

STAINLESS STEEL 304 RING

STAINLESS STEEL 304  PROFILE

STAINLESS STEEL 304  BENDING ANGLE

STAINLESS STEEL 304 BENDING  CHANNELS

STAINLESS STEEL 304L SHEET

STAINLESS STEEL 304L PLATE

STAINLESS STEEL 304 L COIL

STAINLESS STEEL 304L  STRIP

STAINLESS STEEL 304L FLAT

STAINLESS STEEL 304L SHIM

STAINLESS STEEL 304L CIRCLE

STAINLESS STEEL 304L RING

STAINLESS STEEL 304 L PROFILE

STAINLESS STEEL 304 L BENDING ANGLE

STAINLESS STEEL 304L BENDING CHANNELS

Stainless Steel Sheet Finishes

HR {HOT ROLED}  PLATE

2B (Bright, Cold Rolled) SHEET

No. 3 (Brushed, 120 Grit) SHEET

No. 4 (Brushed, 150 Grit) SHEET

No. 8 (Mirror) SHEET

BA (Bright Annealed) SHEET

MATT PVC SHEET

BA PVC SHEET

MIRROR  PVC SHEET

NO8 FINISH SHEET

MATT PVC COIL

BA PVC COIL

MIRROR  PVC COIL

NO8 FINISH COIL

 

Technical data

Chemical Composition

 

C

Si

Mn

P

S

Ni

Cr

Mo

N

SUS304

0.08

0.75

2.00

0.045

0.030

8.50-10.50

18.00-20.00

0.10

SUS304L

0.030

1.00

2.00

0.045

0.030

9.00-13.00

18.00-20.00

304H

0.030

0.75

2.00

0.045

0.030

8.00-10.50

18.00-20.00

-

-

Possible Alternative Grades

Grade

Why it might be chosen instead of 304

301L

A higher work hardening rate grade is required for certain roll formed or stretch formed components.

302HQ

Lower work hardening rate is needed for cold forging of screws, bolts and rivets.

303

Higher machinability needed, and the lower corrosion resistance, formability and weldability are acceptable.

316

Higher resistance to pitting and crevice corrosion is required, in chloride environments

321

Better resistance to temperatures of around 600-900 °C is needed…321 has higher hot strength.

3CR12

A lower cost is required, and the reduced corrosion resistance and resulting discolouration are acceptable.

430