ALLOY 20 PLATE
Alloy 20 Stainless Steel
RMD inventory now includes Alloy 20 (UNS N08020) in sheet, sheet coil, plate, round bar, processed flat bar and tubular products.
GENERAL PROPERTIES Alloy 20 (UNS N08020) is an austenitic, nickel-iron-chromium based super alloy with additions of Copper and Molybdenum which provide resistance to hostile environments, pitting, and crevice corrosion. It is also stabilized with Columbium to minimize carbide precipitation during welding. Alloy 20 appears to fall between both the stainless and nickel categories as it contains characteristics of both. It was designed for maximum resistance to acid attack and demonstrates superior resistance to stress-corrosion cracking in boiling 20% to 40% sulfuric acid, and also has excellent general corrosion resistance to sulfuric acid and to chloride stress corrosion cracking. Alloy 20 has good mechanical properties at both ambient and elevated temperatures, up to approximately930°F (500°C) and is readily fabricated by usual industrial processes.
Specifications: UNS N08020
APPLICATIONS: Alloy 20 was originally designed for use in sulfuric acid related applications; however, it is now frequently used in a wide variety of industries. Applications that commonly use Alloy 20 include:
· Chemical and allied industries
· Food and dye production
· Heat exchangers
· Explosives
· Tanks
· Valves
· Pickling racks
· Manufacture of synthetic rubber and plastics
· Pharmaceuticals
· SO2 scrubbers and other severe environments
STANDARDS:
· ASTM/ASME: UNS N08020
· EURONORM: FeMi35Cr20Cu4Mo2
· DIN: 2.4660
Chemical Properties:
TYPE | C | Cr | Cu | Fe | Mn | Mo | Ni | P | Si | S | Nb(Cb) |
Alloy 20UNSN08020 | 0.07max | min: 19.00max: 21.00 | min: 3.00max: 4.00 | Balance | 2.00max | min: 2.00max: 3.00 | min: 32.00max: 38.00 | 0.045max | 1.00max | 0.035max | 8 XC min1.00 max |